| L2-10007-P SuperVac® Lead Bromide, PbBr2, -80 mesh, 99.9% pure | Evaporation Techniques | |||||
| Density g/cm3 | 6.66 | Crucible | ||||
| Melting Point °C | 373 | Coil | ||||
| E-Beam | Boat | |||||
Qty in grams: | Index of Refraction @ microns | |||||
| L2-10006-P SuperVac® Lead Bromide, PbBr2, -80 mesh, 99.999% pure | Evaporation Techniques | |||||
| Density g/cm3 | 6.66 | Crucible | ||||
| Melting Point °C | 373 | Coil | ||||
| E-Beam | Boat | |||||
Qty in grams: | Index of Refraction @ microns | |||||
| L2-10009-P SuperVac® Lead Chloride, PbCl2, -80 mesh, 99.9% pure | Evaporation Techniques | |||||
| Density g/cm3 | 5.85 | Crucible | Al2O3 | |||
| Melting Point °C | 501 | Coil | ||||
| E-Beam | Boat | Mo | ||||
![]() | Qty in grams: | Index of Refraction @ microns | 2.3 @ 0.55, 2.0 @ 10 | |||
| L2-10008-P SuperVac® Lead Chloride, PbCl2, -80 mesh, 99.999% pure | Evaporation Techniques | |||||
| Density g/cm3 | 5.85 | Crucible | Al2O3 | |||
| Melting Point °C | 501 | Coil | ||||
| E-Beam | Boat | Mo | ||||
![]() | Qty in grams: | Index of Refraction @ microns | 2.3 @ 0.55, 2.0 @ 10 | |||
| L2-10010-P SuperVac® Lead Fluoride, PbF2, -100 mesh, 99.999% pure | Evaporation Techniques | |||||
| Density g/cm3 | 8.24 | Crucible | BeO | |||
| Melting Point °C | 822 | Coil | ||||
| E-Beam | Boat | W & Mo | ||||
![]() | Qty in grams: | Index of Refraction @ microns | 1.92 @ 0.3, 1.60 @ 11 | |||
| L2-10011-P SuperVac® Lead Fluoride, PbF2, -325 mesh (typ.≤10 microns), 99.9% pure | Evaporation Techniques | |||||
| Density g/cm3 | 8.24 | Crucible | BeO | |||
| Melting Point °C | 822 | Coil | ||||
| E-Beam | Boat | W & Mo | ||||
![]() | Qty in grams: | Index of Refraction @ microns | 1.92 @ 0.3, 1.60 @ 11 | |||
| L2-10015-P SuperVac® Lead Molybdate, PbMoO4, -200 mesh, 99.9% pure | Evaporation Techniques | |||||
| Density g/cm3 | Crucible | |||||
| Melting Point °C | Coil | |||||
| E-Beam | Boat | |||||
Qty in grams: | Index of Refraction @ microns | |||||
| L2-10016-P SuperVac® Lead Niobate, PbNb2O6, -200 mesh, 99.9% pure | Evaporation Techniques | |||||
| Density g/cm3 | Crucible | |||||
| Melting Point °C | Coil | |||||
| E-Beam | Boat | |||||
Qty in grams: | Index of Refraction @ microns | |||||
| L2-10017-P SuperVac® Lead Nitrate, Pb(NO3)2, -50 mesh, 99.999% pure | Evaporation Techniques | |||||
| Density g/cm3 | Crucible | |||||
| Melting Point °C | Coil | |||||
| E-Beam | Boat | |||||
Qty in grams: | Index of Refraction @ microns | |||||
| L2-10020-P SuperVac® Lead Oxide, Pb3O4, -100 mesh, 99.9% pure | Evaporation Techniques | |||||
| Density g/cm3 | Crucible | |||||
| Melting Point °C | Coil | |||||
| E-Beam | Boat | |||||
Qty in grams: | Index of Refraction @ microns | |||||
| L2-10018-P SuperVac® Lead Oxide, PbO, -100 mesh, 99.999% pure | Evaporation Techniques | |||||
| Density g/cm3 | 9.53 | Crucible | Quartz & Al2O3 | |||
| Melting Point °C | 890 | Coil | ||||
| E-Beam | Boat | Pt & Mo | ||||
![]() | Qty in grams: | Index of Refraction @ microns | 2.51 @ .59 | |||
| L2-10019-P SuperVac® Lead Oxide, PbO, -325 mesh (typ. ≤10 microns), 99.9% pure | Evaporation Techniques | |||||
| Density g/cm3 | 9.53 | Crucible | Quartz & Al2O3 | |||
| Melting Point °C | 890 | Coil | ||||
| E-Beam | Boat | Pt & Mo | ||||
![]() | Qty in grams: | Index of Refraction @ microns | 2.51 @ .59 | |||
| L2-10022-P SuperVac® Lead Selenide, PbSe, -325 mesh (typ. ≤10 microns), 99% pure | Evaporation Techniques | |||||
| Density g/cm3 | 8.1 | Crucible | Graphite & Al2O3 | |||
| Melting Point °C | 1065 | Coil | ||||
| E-Beam | Boat | W & Mo | ||||
![]() | Qty in grams: | Index of Refraction @ microns | 3.5 @ 1.0 | |||
| L2-10021-P SuperVac® Lead Selenide, PbSe, -325 mesh (typ. ≤10 microns), 99.999% pure | Evaporation Techniques | |||||
| Density g/cm3 | 8.1 | Crucible | Graphite & Al2O3 | |||
| Melting Point °C | 1065 | Coil | ||||
| E-Beam | Boat | W & Mo | ||||
![]() | Qty in grams: | Index of Refraction @ microns | 3.5 @ 1.0 | |||
| L2-10023-P SuperVac® Lead Selenite, PbSeO3, -100 mesh, 99.9% pure | Evaporation Techniques | |||||
| Density g/cm3 | Crucible | |||||
| Melting Point °C | Coil | |||||
| E-Beam | Boat | |||||
Qty in grams: | Index of Refraction @ microns | |||||
| L2-10024-P SuperVac® Lead Suphide, PbS, -200 mesh, 99.9% pure | Evaporation Techniques | |||||
| Density g/cm3 | 7.5 | Crucible | Quartz & Al2O3 | |||
| Melting Point °C | 1114 | Coil | ||||
| E-Beam | Boat | W | ||||
![]() | Qty in grams: | Index of Refraction @ microns | 3.9 @ 0.5 | |||
| L2-10025-P SuperVac® Lead Tantalate, PbTa2O6, -200 mesh, 99.9% pure | Evaporation Techniques | |||||
| Density g/cm3 | Crucible | |||||
| Melting Point °C | Coil | |||||
| E-Beam | Boat | |||||
Qty in grams: | Index of Refraction @ microns | |||||
| L2-10027-P SuperVac® Lead Telluride, PbTe, -325 mesh (typ. ≤10 microns), 99% pure | Evaporation Techniques | |||||
| Density g/cm3 | 8.16 | Crucible | Graphite & Al2O3 | |||
| Melting Point °C | 917 | Coil | ||||
| E-Beam | Boat | Ta & Mo | ||||
![]() | Qty in grams: | Index of Refraction @ microns | 5.6 @ 5, 3.4 @ 30 | |||
| L2-10026-P SuperVac® Lead Telluride, PbTe, -325 mesh (typ. ≤10 microns), 99.99% pure | Evaporation Techniques | |||||
| Density g/cm3 | 8.16 | Crucible | Graphite & Al2O3 | |||
| Melting Point °C | 917 | Coil | ||||
| E-Beam | Boat | Ta & Mo | ||||
![]() | Qty in grams: | Index of Refraction @ microns | 5.6 @ 5, 3.4 @ 30 | |||
| L2-10028-P SuperVac® Lead Tellurite, PbTeO3, -100 mesh, 99.9% pure | Evaporation Techniques | |||||
| Density g/cm3 | Crucible | |||||
| Melting Point °C | Coil | |||||
| E-Beam | Boat | |||||
Qty in grams: | Index of Refraction @ microns | |||||
| L2-10029-P SuperVac® Lead Titanate, PbTiO3, -325 mesh (typ. ≤10 microns), 99.9% pure | Evaporation Techniques | |||||
| Density g/cm3 | 7.52 | Crucible | ||||
| Melting Point °C | Coil | |||||
| E-Beam | Boat | Ta | ||||
![]() | Qty in grams: | Index of Refraction @ microns | ||||
| L2-10030-P SuperVac® Lead Tungstate, PbWO4, -200 mesh, 99.9% pure | Evaporation Techniques | |||||
| Density g/cm3 | Crucible | |||||
| Melting Point °C | Coil | |||||
| E-Beam | Boat | |||||
Qty in grams: | Index of Refraction @ microns | |||||
| L2-10031-P SuperVac® Lead Vanadate, PbV2O6, -200 mesh, 99.9% pure | Evaporation Techniques | |||||
| Density g/cm3 | Crucible | |||||
| Melting Point °C | Coil | |||||
| E-Beam | Boat | |||||
Qty in grams: | Index of Refraction @ microns | |||||
| L2-10032-P SuperVac® Lead Zirconate, PbZrO3, -325 mesh (typ. ≤10 microns), 99.7% pure | Evaporation Techniques | |||||
| Density g/cm3 | Crucible | |||||
| Melting Point °C | Coil | |||||
| E-Beam | Boat | |||||
Qty in grams: | Index of Refraction @ microns | |||||